High Performance
Steel Meeting
The full penetration welding of this three foot long plate with
two inch thickness takes only 16 minutes with the new Narrow Gap
Improved Electroslag Weld compared to six hours with the conventional
method.


Bob Turpin of the Oregon Graduate Institute demonstrates to onlookers
what it takes to produce a weld using the narrow Gap Improved Electroslg
Weld.

|